Ntau qhov tsis xws ntawm vuam
01. Ncaim
Yog tias cov txheej txheem vuam tsis raug xaiv los yog kev ua haujlwm tsis yog tus qauv, cov grooves los yog kev nyuaj siab tsim nyob rau hauv lub hauv paus hlau thaum vuam yog hu ua undercuts.
Thaum koj thawj zaug pib vuam, vim koj tsis paub qhov loj ntawm qhov tam sim no thiab koj txhais tes tsis ruaj khov thaum lub sij hawm vuam, nws yooj yim los ua undercuts. Txhawm rau tiv thaiv undercuts, koj yuav tsum tau xyaum ntau cov txheej txheem vuam. Koj yuav tsum nyob ruaj khov thiab tsis txhob ua siab ntev.
Xinfa vuam cov cuab yeej muaj cov yam ntxwv zoo thiab tus nqi qis. Yog xav paub ntxiv, thov mus saib:Vuam & txiav Manufacturers - Tuam Tshoj Vuam & Txiav Hoobkas & lwm tus neeg (xinfatools.com)

Nov yog daim duab ntawm lub undercut
02. Stomata
Thaum lub sij hawm vuam, cov roj hauv lub pas dej molten tsis khiav tawm thaum lub sij hawm khov, thiab cov kab noj hniav tsim los ntawm cov seem hauv cov vuam yog hu ua pores.
Thaum pib ntawm vuam, vim tsis muaj peev xwm ua tau zoo ntawm kev sib dhos vuam thiab txoj kev tsis muaj peev xwm ntawm kev thauj cov strips, nws yuav ua rau ncua, sib sib zog nqus thiab ntiav, uas tuaj yeem yooj yim ua rau qhov pores. Txoj hauv kev los tiv thaiv nws tsis yog ua siab ntev thaum vuam, tuav koj tus kheej txoj haujlwm, thiab nqa tawm cov strips ib kauj ruam. Qhov tseeb, nws yog tib yam li kev sau ntawv calligraphy. , ib yam li kev sau ntawv, mob stroke los ntawm mob stroke.

Qhov no yog qhov vuam qhov
03. Tsis nkag mus, tsis fused
Muaj ntau qhov laj thawj rau kev vuam tsis tiav thiab tsis tiav fusion, xws li: qhov sib txawv los yog zawj lub kaum sab xis ntawm lub vuam yog me me dhau, qhov blunt ntug tuab heev, txoj kab uas hla ntawm vuam pas nrig loj dhau, qhov vuam ceev dhau los yog lub arc ntev dhau lawm, thiab lwm yam. Cov nyhuv vuam kuj tseem tuaj yeem cuam tshuam los ntawm qhov muaj impurities hauv qhov zawj, thiab cov impurities unmelted kuj tseem tuaj yeem cuam tshuam cov nyhuv fusion ntawm vuam.
Tsuas yog thaum vuam, tswj qhov vuam ceev, tam sim no thiab lwm yam txheej txheem tsis, xaiv qhov zawj loj, thiab tshem tawm cov nplai oxide thiab impurities ntawm qhov zawj; cov welding hauv qab yuav tsum tau meej.

Tsis nkag mus
04. Kub dhau
Thaum lub sij hawm vuam txheej txheem, cov hlau molten ntws tawm ntawm lub nraub qaum ntawm qhov zawj, tsim ib qho kev tsis xws luag hu ua hlawv-dhau.
Txoj hauv kev los tiv thaiv nws yog kom txo qhov tam sim no thiab txo qhov sib txawv ntawm qhov vuam.

Vuam duab hlawv dhau
05. Lub vuam nto tsis zoo nkauj
Piv txwv li, qhov tsis xws luag xws li kev sib tshooj thiab serpentine weld hlaws yog tshwm sim los ntawm qhov vuam ceev qeeb dhau thiab qhov vuam tam sim no qis dhau.
Txoj hauv kev los tiv thaiv nws yog kev xyaum ntau dua thiab paub qhov tsim nyog vuam ceev. Cov neeg feem coob ua qhov no thaum pib, xyaum ntau dua.

Serpentine weld hlaws

sib tshooj weld